An equipment foundation is only as good as the layer between the concrete and the steel. A machine can be levelled perfectly and still sit on a poorly filled bed. That layer is where construction grout does its work: it fills the space under the baseplate, holds the plate in firm contact with the foundation and passes operating loads into the concrete. For engineers and contractors in Sri Lanka planning pump sets, compressors, generators or column bases, the practical questions are always the same. Will the grout flow into every corner? Will it stay filled once it sets? How will we know the baseplate is properly supported?
This guide answers those questions using Redwop’s published information on its non-shrink grout range. It does not repeat Redwop’s general articles on grout types and uses or on why cementitious grouts crack or shrink. Its focus is narrower: flow, void filling and the checks around a baseplate. Where Redwop’s pages do not publish a figure, such as a specific flow value for each product, this article says so and points to the datasheet.
On This Page
- What construction grout does under a baseplate
- Grout flow and workability
- Void filling beneath equipment baseplates
- Non shrink grout for steel columns
- Non Shrink Grout Under Base Plate: preparation, mixing, placement and curing
- Redwop’s non-shrink range: what the pages publish
- Cement-based or epoxy-based: choosing the grout family
- Baseplate inspection checklist
- Common mistakes and precautions
- Grouting equipment foundations in Sri Lanka
- Information to send for an enquiry
- Frequently asked questions
- Final Thoughts
What construction grout does under a baseplate
A baseplate does not rest directly on a perfectly flat foundation. There is always a gap, often created deliberately so the plate can be levelled. Construction grout fills that gap. Redwop describes its Non Shrink Grout as designed for secure load transfer between structural elements, and its product pages list machine base plates, anchor bolts, precast elements, bridge bearings and column foundations among the applications.
The word “non-shrink” matters here. Redwop says its grout is engineered to maintain volume during curing, so that it keeps intimate contact between the plate and the foundation. A grout that loses volume as it sets can leave a thin gap under the plate, which is the opposite of what the layer is there to do. This is why non shrink grout, rather than an ordinary cement mortar, is the usual reference point for equipment bases.
The layer also has to work under the equipment’s own behaviour. Redwop’s product pages mention static and dynamic loads, and describe the grout as providing support to bearing areas and dampening vibration. A pump or compressor produces repeated forces every time it runs, so the bed beneath it has to remain in contact with the plate over the long term, not just on the day of grouting.
Grout flow and workability
Flow is what allows the grout to reach the far side of a wide baseplate or the inside of a bolt pocket without being forced. Redwop’s non-shrink pages describe the material as free flowing, with consistency adjustable on site. The Non Shrink Grout application guide says to mix water suggested in datasheet per 25 kg bag until the mix is smooth and lump-free, to use less water for a dry-pack and more for a pourable mix.Three points follow from this.
- Water is the adjustment, so it needs control. Add it by measure for each bag, not by eye, and keep the same water for every batch in one pour so the consistency does not change midway.
- Place immediately after mixing. Redwop’s guide says to apply the grout straight away and to pour continuously.
- Choose the consistency for the job. A pourable mix suits a baseplate with a clear pouring route. A stiffer dry-pack suits post bases and tight spots, where Redwop says to use a mortar bag or pack by hand firmly.
Redwop also says the grout can be pumped at a pourable consistency, with continuous placement and air excluded on deep fills. For deeper sections, the guide names tremie or pump placement to prevent air entrapment.
One limit applies. Redwop’s pages describe the grout as suitable for joints up to 100 mm, and the category FAQ confirms this. The pages do not publish a separate flow figure in the text, so any flow requirement in a specification should be checked against the product datasheet (for example ARACONE AT, ARACONE GR45 and GR65).
| Placement approach | Water guidance on the Redwop page | What to confirm |
|---|---|---|
| Pourable | About 4L (0.16 W/P) per 25 kg bag (FAQ) | Datasheet flow value and working time |
| Pumped or tremie for deep fills | Pourable consistency, continuous placement | Pump type and a route that excludes air |
| Dry-pack | Less water than pourable | Packing method for post bases and tight spots |
Void filling beneath equipment baseplates
A void under a baseplate means part of the plate is not supported. Redwop’s product pages address this directly. ARACONE AT is described as ensuring a high level of contact with load-bearing areas and helping complete filling without voids, with no need for external aids such as rodding, poking or chaining. ARACONE GR45 is described as providing complete filling without voids and dampening vibration.
What these statements do not do is remove the need for good site practice. Redwop’s own application guide gives the practical points that reduce the risk of voids:
- Pour continuously, with no pause that lets one batch start to set before the next arrives.
- Use tremie or pump placement for deep fills to prevent air entrapment.
- Maintain continuous grout flow at the ends and taper edges with a margin trowel.
The areas that need attention are the ones the grout has to reach last: the far side from the pouring point, the corners of the plate and the surrounds of anchor bolts. Where a pour has to run across a wide plate, plan the feed side and the receiving side in advance so grout moves in one direction and displaces air ahead of it.
Redwop does not publish a method for detecting a void after the grout has set. That inspection method, and the acceptance criteria, belong in the project specification and should be agreed with the structural engineer before grouting begins.
Non shrink grout for steel columns
Steel column bases face the same gap between plate and concrete, usually on a pedestal. Redwop’s Non Shrink Grout page lists precast column bases and column foundations among its applications, and describes the product as ensuring firm bedding and accurate load transfer without settlement. The application guide also covers dry-packing for post bases.
For non shrink grout for steel columns, the points that matter most are those where the column differs from a machine:
- The column load is vertical and sustained, so the full plate area needs bedding.
- The grout space is often narrow, so the choice between a pourable and a dry-pack mix depends on the access to each side of the plate.
- Leveling nuts or shims hold the plate at height. Plan their position before grouting so the pour is not obstructed.
Redwop notes that its Non Shrink Grout has a non-ferrous, non-corrosive formulation so that steel surfaces remain protected from rust. ARACONE AT and GR45 make similar statements about not causing corrosion of machine parts and anchor bolts.
Non Shrink Grout Under Base Plate: preparation, mixing, placement and curing
This section pulls together what Redwop publishes for the grouting sequence in Non Shrink Grout Under Base Plate work. It is the published guidance, not a full method statement.
Preparation
Redwop’s pages for the non-shrink range do not list a detailed surface preparation procedure for foundations. The Non Shrink Grout page and the product pages for ARACONE AT, GR45 and GR65 do not describe foundation surface preparation or formwork. That information should come from the datasheet, from Redwop’s technical team and from the project engineer. Record the preparation method agreed for the foundation surface and the containment around the plate before work starts.
Mixing
The published guide is simple: water in the stated range per 25 kg bag, mixed to a smooth, lump-free consistency, adjusted for the placement method. Redwop’s coverage calculator is available on its site for quantity estimates.
Placement
Place immediately after mixing and keep the flow continuous. For deeper sections use tremie or pump placement. For post bases, hand-pack tightly with a mortar bag. Taper the edges with a margin trowel.
Curing and loading
The guide says to wet-cure for at least 24 hours under protected conditions. The FAQ adds that the grout supports light loads in 24 hours, develops full strength in 7 days and reaches optimal properties at 28 days. It also says the grout typically achieves more than 70 MPa after 28 days per ASTM C109. Redwop warns against extreme heat and freezing. Use these timings to plan when equipment can be bolted down and run, but confirm them against the datasheet for the specific product.
| Stage | Published guidance | Verify before use |
|---|---|---|
| Mix | About 3.5 to 4L(0.16 W/P) per 25 kg bag | Datasheet water range for the chosen product |
| Placement | Immediately after mixing; continuous pour; tremie or pump for deep fills | Gap depth and pouring route |
| Finishing | Taper edges with a margin trowel | Edge detail agreed with the engineer |
| Curing | Wet-cure at least 24 hours, protected | Curing method on site |
| Loading | Light loads at 24 hours; full strength at 7 days | Datasheet and engineer’s release criteria |
Redwop’s non-shrink range: what the pages publish
Redwop lists three cement-based non-shrink grouts under its Non Shrink Grout product, plus related pourable and expanding products. They are not identical, and the pages should not be treated as interchangeable.
| Product | What the page says | Listed uses |
|---|---|---|
| ARACONE AT | Free-flowing, ready-to-use powder; very low water requirement; controlled expansion to retain original volume; no segregation or bleeding | Base plates and bolt pockets of turbo generators, diesel generating sets, crane and transporter rails, compressors, pump sets, pulverizing mills, rolling mill beds, and cement, textile, granite and paper plant machinery |
| ARACONE GR45 | Free-flowing; micro-cellular structure with high frost, fire and oil resistance when set; low water demand | Heavy-duty support beneath load-bearing structure; transfer of operational loads to the foundation |
| GR65 | Free-flowing precision grout; gaseous expansion system compensates for shrinkage and settlement in the plastic state; no metallic iron | Precision grouting under static and dynamic loads; base plates of turbines, compressors, boiler feed pumps; anchoring masts, anchor bolts, fence posts |
| Non Shrink Grout | Fibre-reinforced, cementitious, chloride-free; pourable or dry-pack | Machine base plates, anchor bolts, precast elements, bridge bearings, column foundations |
The Expanding Grout page describes a cementitious grout with slight positive expansion, adjustable from plastic to flowable, placed by pouring, pumping or hand-packing, with typical compressive strengths of 50 to 80 MPa. Note that it states the product contains no corrosive fibers or chlorides, while the Non Shrink Grout page describes a fibre-reinforced product, so check the datasheet for the exact formulation of the grade you intend to use.
Cement-based or epoxy-based: choosing the grout family
Not every baseplate calls for a cementitious grout. Redwop’s Epoxy Based Pourable Grout and REP 65CM are three-component epoxy systems of resin, hardener and filler, described for free-flow grouting of gaps from about 5 to 120 mm. Redwop lists reciprocating machinery, turbine beds, heavy crane rails and chemical plants among the uses, and cites low creep, resistance to continuous dynamic loads and chemical resistance. Its comparison of epoxy and cement grout covers the wider trade-offs.
| Consideration | Cement-based non-shrink | Epoxy-based pourable |
|---|---|---|
| Components | Powder plus water | Resin, hardener and filler |
| Gap range on Redwop pages | Up to 100 mm | About 5 to 120 mm |
| Flagged strengths | Expansion or volume stability; high early and final strength | Low creep; chemical resistance; dynamic loads |
| Where the page points | General machinery and column bases | Chemical spillage, heavy dynamic loads, process plants |
Treat this as a starting point for a conversation with the engineer. The choice should follow the loading, the chemical exposure and the specified gap, and the datasheet should settle it.
Baseplate inspection checklist
Redwop does not publish an inspection procedure for baseplate grouting. The checks below are project verification items, grouped by stage, that a site team can agree with the engineer. They are not Redwop test methods.
| Stage | Check | Record |
|---|---|---|
| Before grouting | Foundation surface prepared as specified | Method and date |
| Before grouting | Plate level and position fixed, leveling devices placed | Survey readings |
| Before grouting | Containment around the grout space complete | Photograph |
| During grouting | Water measured per bag; batches consistent | Bags used, water per bag |
| During grouting | Pour continuous; one feed direction; air excluded | Start and finish times |
| After grouting | Edges tapered and finished | Photograph |
| After grouting | Wet-curing started and kept protected | Curing log, at least 24 hours |
| Before loading | Release agreed against datasheet timings | Engineer’s sign-off |
Common mistakes and precautions
The table follows the layout used in Redwop’s other guides and ties each point to published guidance or marks it for verification.
| Issue | Technical approach | Verification |
|---|---|---|
| Water added by eye | Measure water per bag within the published range | Record water per bag |
| Pour interrupted | Pour continuously; plan the feed side first | Pour log |
| Air trapped in deep fills | Use tremie or pump placement | Method statement |
| Wrong product for the duty | Match the product to load, gap and exposure | Datasheet check |
| Thick gap beyond published range | Do not exceed the stated limit | Gap survey against the page |
| Early loading | Wait for the release timing; light loads at 24 hours only | Engineer’s release |
| Poor curing | Wet-cure at least 24 hours, protected | Curing log |
| Assuming all non-shrink grouts are alike | Read each product’s own page and datasheet | Product comparison on file |
The most useful habit is to treat every number in this article as a prompt to check the datasheet, not as a substitute for it.
Grouting equipment foundations in Sri Lanka
Redwop maintains a Sri Lanka page and has published Sri Lanka-focused material, including its guide to interior wall waterproofing in Sri Lanka. This article does not cite local standards, regulations or project examples, because Redwop’s pages do not provide them, and it makes no claims about how the products perform in Sri Lankan conditions.
What can be said is practical. The industrial plant listed on Redwop’s ARACONE AT page (cement, textile, granite, paper and rolling mill machinery, pulverizing mills and generating sets) is the kind of equipment found in industrial projects generally. Contractors should select the grout against the equipment’s load, the baseplate gap and the site’s own requirements, then confirm supply, documentation and delivery with Redwop for the project location. Redwop describes itself as a manufacturer, exporter and supplier, so datasheets and technical support can be requested directly.
Information to send for an enquiry
To receive a useful product recommendation, send Redwop the equipment type and weight, the baseplate dimensions, the grout gap thickness, the loading (static or dynamic), any chemical or oil exposure, the pouring and access arrangement, the number of bases and the project location. Ask for the datasheet and safety data sheet of the proposed grade, and confirm packaging, lead time and the quantity calculation before ordering.
Frequently asked questions
What is construction grout used for in equipment foundations?
It fills the gap between the concrete foundation and the baseplate so the plate is fully supported and loads pass into the foundation.
Why is non-shrink grout used beneath baseplates?
Redwop says its non-shrink grout is designed to maintain volume during curing, which keeps contact between the plate and the concrete.
What is the purpose of non-shrink grout for steel columns?
It beds the column baseplate on its pedestal, giving firm support and load transfer. Redwop lists precast column bases and column foundations among its applications.
Why does grout flow matter?
A free-flowing mix can reach the far side of a plate and around bolts. Redwop adjusts flow with the amount of water per bag.
How can voids affect support?
An unfilled area under a plate is unsupported. Redwop’s pages say its grouts are designed for complete filling, but placement still has to be continuous.
What preparation is needed before applying the grout?
Redwop’s pages do not give a detailed foundation preparation method. Follow the datasheet and the engineer’s specification.
How do I check that grout has filled the space?
Agree the inspection approach and acceptance criteria with the engineer before work begins.
What should I consider when selecting a non-shrink grout?
The load, the gap, the exposure and the product’s own datasheet. The pages show differences between ARACONE AT, GR45, GR65 and the epoxy options.
How important is curing?
Redwop says to wet-cure for at least 24 hours under protected conditions, and gives light loading at 24 hours and full strength at 7 days.
What should be checked before accepting the grouting work?
Level and position records, water per bag, a continuous pour log, the curing record and the engineer’s release against the datasheet.
Final Thoughts
Grouting an equipment foundation is a short job that carries a long consequence. The layer under the baseplate has to flow into every corner, stay filled and keep its contact as the equipment runs. Redwop’s published guidance supports a clear approach: choose a product whose page matches the duty, mix by measured water, place continuously, avoid trapped air, wet-cure and release the equipment against the datasheet.
What the pages do not publish matters just as much. There is no foundation preparation method, no void detection test and no flow figure on the web pages, so these belong in the project specification and the datasheets. For Sri Lankan projects, send Redwop the equipment, gap and loading details through its contact page and request the datasheets for the grade you intend to use. Redwop’s wider grouts range lists the other options.
Tags: Construction Grout, Non Shrink Grout, Equipment Foundations, Baseplate Grouting, Construction Chemicals Sri Lanka